Table 1: Material property for the liquid fuel (kerosene) and the composite material.
Property |
Kerosene |
Composite material |
Conductivity, k (W/m.K) |
0.17 |
0.515 |
Density, (kg/m3) |
750 |
1625 |
Heat capacity, Cp (kJ/kg.K) |
2.45 |
2.015 |
Pyrolysis heat, Lv (kJ/kg) |
256 |
9800 |
Combustion heat, Hc (kJ/kg) |
44000 |
21000 |
Boiling temperature, TB (℃) |
216 |
- |
Ignition temperature, TIgn (℃) |
- |
390 |
Surface emissivity, |
1 |
0.9 |